3M Scotch® 214 High-Temperature Masking Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 214 High-Temperature Masking Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® High Temperature Masking Tape 214 is good for one hour at 350°F (177°C) on most surfaces. The adhesive is sulfur-free which makes it one of the few tapes that can be used on copper, silver and other precious metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 4.42 microns
0.174 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.7 MPa
4740 psi
ASTM D3759
Elongation at Break 10 %
10 %
ASTM D3759
Peel Strength 0.31773 kN/m
1.8125 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Descriptive Properties Value Comments
Adhesive Type Firm rubber adhesive