3M Safety-Walk™ 310 Black Slip-Resistant Medium Resilient Tapes and Treads

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Safety-Walk™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Safety-Walk™ 310 Black Slip-Resistant Medium Resilient Tapes and Treads.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft-textured, non-mineral, medium resilient surface bonded to a pressure-sensitive adhesive backed plastic film. For barefoot- or shoe-traffic areasNon-mineral, medium textured, slip-resistant vinyl surfaceTextured resilient high friction surface and durable adhesive provide long-lasting performanceApplications: locker rooms, around hot tubs and pools, boats, personal watercraft, water skis, exercise equipment conveyersInformation provided by 3M
Physical Properties Metric English Comments
Thickness 1140 microns
45.0 mil
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 79.0 °C
174 °F
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Descriptive Properties Value Comments
Appearance Black