Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M RPF-CWR (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass with Woven Roving

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M RPF-CWR (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass with Woven Roving.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ RPF-C (Reinforced Polyurethane Foam) is a polyurethane foam with layers of continuous strand fiberglass and woven roving throughout the polyurethane. The composites are 30% to 45% lighter than plywood, have a high strength-to-weight ratio, very low water absorption (1.0% or less) and will not have any water rot or insect infestation.Information provided by 3M
Physical Properties Metric English Comments
Water Absorption 1.1 %
1.1 %
ASTM C272
Mechanical Properties Metric English Comments
Flexural Strength 21.7 MPa
3150 psi
ASTM D790
Flexural Modulus 1.427 GPa
206.9 ksi
ASTM D790
Compressive Strength 5.89 MPa
854 psi
Core; ASTM C365
Compressive Modulus 0.18004 GPa
26.113 ksi
Core; ASTM C365
Shear Modulus 0.02711 GPa
3.932 ksi
Core; ASTM C273
Shear Strength 2.85 MPa
414 psi
Core; ASTM C273