Material Notes:
3M™ Novec™ Electronic Degreaser is a strong non-flammable cleaner ideal for removal of heavy oils, greases and handling soils from internal components of electronic equipment, precision devices and other electromechanical or sensitive devices.Features and Benefits:Non-flammableFast drying, no residueLow odorNon-corrosiveLow toxicityCompliant with CARB and OTC VOC regulationsContains no NCFCs, HFCs, nPB or HAPsNon-ozone depletingInformation provided by 3M
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
Surface Tension 19 dynes/cm
19 dynes/cm
Electrical Properties Metric English Comments
Dielectric Strength >= 0.984 kV/mm
>= 25.0 kV/in
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Users viewing this material also viewed the following: