Material Notes:
Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 and do not contain glassy phases. This allows the fibers to retain their strength at high temperatures. 3M Nextel Fiber 720, an alpha-Al2O3 with SiO2 addition (forming alpha-Al2O3/mullite), has improved strength retention at temperature due to reduced grain boundary sliding. The SiO2 addition also help to 'pin' the grains and reduce grain growth when exposed to thermal aging.Information provided by 3M Ceramic Textile and Composites.
Physical Properties Metric English Comments
Density 3.40 g/cc
0.123 lb/in³
Particle Size <= 0.50 µm
<= 0.50 µm
Crystal size
Specific Surface Area <= 0.20 m²/g
<= 0.20 m²/g
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2100 MPa

@Thickness 25.4 mm
305000 psi

@Thickness 1.00 in
gauge filament
Modulus of Elasticity 260 GPa
37700 ksi
Filament in Tension
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Temperature 100 - 1100 °C
3.33 µin/in-°F

@Temperature 212 - 2010 °F
Melting Point 1800 °C
3270 °F
Optical Properties Metric English Comments
Refractive Index 1.67
1.67
Descriptive Properties Value Comments
Color Green
Users viewing this material also viewed the following: