3M Hi-Strength 90 Spray Adhesive (Bulk)

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Hi-Strength
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Hi-Strength 90 Spray Adhesive (Bulk).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An industrial grade spray adhesive that is typically used for bonding HPL to woodFeatures:A high strength, fast, contact-type adhesiveExcellent adhesive for decorative laminates, particleboard, and many other materials, even polyethylene, polypropylene, and SBR rubberHas excellent heat resistanceInformation provided by 3M
Physical Properties Metric English Comments
Density 0.767 g/cc
0.0277 lb/in³
Solids Content 23 %
23 %
Volatile Organic Compounds (VOC) Content 356 g/l
356 g/l
Descriptive Properties Value Comments
Appearance Translucent
Base Synthetic Elastomer