Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M GM400 Gripping Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M GM400 Gripping Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Gripping Material GM400 is based on 3M’s proprietary micro-replicated technology. 3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM 110 consists of a high-friction surface with a nylon knit backing that provides stretch in the cross-web direction. It can be attached to other substrates by sewing. 3M gripping material GM110 is ideally suited for applications requiring stretch, such as athletic gloves. When used alone on a single surface 3M gripping material provides a strong secure grip. Then used as a two-part system, for example on a glove and a handlebar grip, strength is maximized. As firmly as 3M gripping material holds, it releases just as easilyInformation provided by 3M
Physical Properties Metric English Comments
Thickness 838 microns
33.0 mil
without liner
940 microns
37.0 mil
with liner
Mechanical Properties Metric English Comments
Coefficient of Friction 3.0

@Pressure 0.0207 MPa
3.0

@Pressure 3.00 psi
dry, kinetic, contact area: 2.8 cm<sup>2</sup>
3.0

@Pressure 0.0207 MPa
3.0

@Pressure 3.00 psi
wet, kinetic, contact area: 2.8 cm<sup>2</sup>
Tear Strength 18.75 kN/m
107.1 pli
MD; ASTM D5734
25.0 kN/m
143 pli
CD; ASTM D5734
Abrasion 0.050
0.050
H18, 500g, weight loss rate at 4000 revolutions; ASTM D3389
>= 6000
>= 6000
H18, 500g, through- revolutions weight loss; ASTM D3389
Film Tensile Strength at Break, MD 3.96 MPa
574 psi
ASTM D5035
Film Tensile Strength at Break, TD 3.76 MPa
545 psi
ASTM D5035
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.0 °C
160 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Adhesive Carrier Polyester mesh
Appearance Black
Users viewing this material also viewed the following: