3M FIP 1-Step Fire Barrier Rated Foam

Category Other Engineering Material
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FIP 1-Step Fire Barrier Rated Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Fire Barrier Rated Foam (FIP 1-Step), is a smoke, sound, and firestopping foam for wall and floor penetrations. Premium two-part, easy-to-handle formulations. Expands up to five times during installation and bonds to most construction substrates including, but not limited to, concrete, metal, wood, plastic and cable jacketing. Dries to a flexible solid. During a fire, product maintains a tight firestop against smoke and flame.Information provided by 3M
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 250 g/l
<= 250 g/l
VOC Less H2O and Exempt Solvents
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Processing Properties Metric English Comments
Cure Time 1.00 min
0.0167 hour
Tack-free
2.00 min
0.0333 hour
Full
Descriptive Properties Value Comments
Appearance Maroon