3M FC-4400 Ionic Liquid Antistatic

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FC-4400 Ionic Liquid Antistatic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Ionic Liquid Antistatic FC-4400 is a high purity antistatic additive compatible with a variety of high performance polymer systems.Features and Benefits:Optical ClarityNo metal or halogen ionsVery low water solubility provides for excellent antistatic durabilityStatic dissipation in wide variety of polymers with typical resistivities of 109 to 1012 ohms/sqThermal stability with a TGA trigger temperature of 429 CWide liquid range for ease of handling in productionInformation provided by 3M
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Volatiles <= 0.10 %
<= 0.10 %
pH 5.0
5.0
neutral
Viscosity 531 cP
531 cP
supercooled
Thermal Properties Metric English Comments
Melting Point 27.5 °C
81.5 °F
Descriptive Properties Value Comments
Appearance Clear colorless liquid or white crystalline solid
Solubility 765 ppm
in water