3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.Modified PTFE fine powder product for paste extrusion applications. The modified PTFE paste extrusion grade, TFM 2001, combines the traditional attributes of first generation PTFE with benefits such as denser polymer structure and lower permeability; uniform mechanical properties; higher stress cracking resistance; higher pressure resistance under surge stress; and weldability. Dyneon TFM 2001 PTFE is an ideal material for the manufacture of high-performance tubing for hydraulic systems, fuel lines, flexible lines, conveying and transport tubing. Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.15 g/cc
0.0777 lb/in³
ASTM D4895
Apparent Bulk Density 0.450 g/cc
0.0163 lb/in³
DIN 53466
Particle Size 500 µm
500 µm
ASTM D4895
Thickness 1600 microns
63.0 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.0 MPa
4930 psi
ASTM D4895
Elongation at Break 400 %
400 %
ASTM D4895
Descriptive Properties Value Comments
Extrusion Pressure 3770 psi
reduction ratio 400; ASTM D4895
Reduction Ratio Range 20-1000:1
Dyneon Method