Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ TF 9205 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer 3M Dyneon™
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 9205 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Dyneon™ PTFE TF micropowders can be used as additives in many different applications and at concentrations typically from 5 to 20%. Homogeneous incorporation helps ensure optimum performance. Because of its small particle size coupled with good free-flowing properties, Dyneon PTFE TF 9205 exhibits very good metering behavior and can be easily incorporated into other materials – even in dry blends.Product Features: Low molecular weight PTFE produced by thermal degradation Rigid particle morphologyUsed as an additive to: Improve non-stick properties Reduce coefficient of friction Increase wear resistance of matrix materialInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D4895
Particle Size 8.0 µm
8.0 µm
average; ISO 13321
Specific Surface Area 2.0 m²/g
2.0 m²/g
BET; DIN 66132
Viscosity 100000 cP
100000 cP
Melt
Melt Flow 12 g/10 min
12 g/10 min
ISO 1133
Thermal Properties Metric English Comments
Melting Point 325 °C
617 °F
Peak Temperature