Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ PVDF 11008/0001 Polyvinylidene Fluoride

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ PVDF 11008/0001 Polyvinylidene Fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries. PVDF is also gaining recognition in automotive, building, electronics, food processing, pharmaceutical and battery applications. PVDF 11008/0001 combines excellent chemical resistance, dimensional stability and excellent flame and smoke resistance with a moderate degree of flexibility. (For applications requiring high degrees of flexibility, see our 30000 series copolymers.) PVDF 11008/0001 has set the standard for plenum rating jacketing and tubes, consistently achieving UL 150°C rating in numerous cable constructions and fiber raceway designs.Features and Benefits:PVDF 11008/0001 is a copolymer of VF2 and HFP (hexafluoropropylene)Improved flexibility over PVDF homopolymersIdeal for applications where high strength and a moderate degree of flexibility are requiredIdeal for high speed extrusionExcellent weatherabilityGood chemical resistanceLong term use temperatures up to 150°C (302ºF) Processable using most conventional thermoplastic conversion techniquesInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ISO 1183
Water Absorption <= 0.040 %
<= 0.040 %
24 hr @ 23°C; ISO 62 (method 1)
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
24 g/10 min

@Load 5.00 kg,
Temperature 230 °C
24 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.0 MPa
6820 psi
50mm/min; ASTM D638
Elongation at Break 600 %
600 %
50mm/min; ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
2mm/min; ASTM D790
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Crystallinity by DSC; ASTM D3418
Descriptive Properties Value Comments
Form Granules