Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, and oil and gas industry, PVDF is also gaining recognition in automotive, building, electronics, pharmaceutical and batteries. 3M™ Dyneon™ PVDF 1008/0001 is easily processed under a variety of conventional thermoplastic conversion techniques, being particularly suitable for injection molding. Dyneon PVDF 1008/0001 is inherently pure and chemically resistant against a variety of aggressive fluids and solvents. PVDF 1008/0001 exhibits excellent dimensional stability, abrasion resistance and high strength, and maintains its mechanical properties at elevated temperature. These products are supplied in pellet form utilizing high purity packaging techniques.Excellent chemical resistance to a variety of aggressive fluids and solventsGood permeation resistanceInjection molding gradeExcellent strength and dimensional stabilityInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ISO 1183
Water Absorption <= 0.040 %
<= 0.040 %
24 hr @ 23°C; ISO 62 (method 1)
Linear Mold Shrinkage 0.030 cm/cm
0.030 in/in
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
24 g/10 min

@Load 5.00 kg,
Temperature 230 °C
24 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.0 MPa
6090 psi
ASTM D638
Tensile Strength, Yield 55.0 MPa
7980 psi
50mm/min; ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
50mm/min; ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
2mm/min; ASTM D790
Thermal Properties Metric English Comments
Melting Point 174 °C
345 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 148 °C
298 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
Flammability, UL94 V-0
V-0
Oxygen Index >= 44 %
>= 44 %
ASTM D2863
Descriptive Properties Value Comments
Form Pellets
Users viewing this material also viewed the following: