Material Notes:
Dyneon PFA 6900GZ is a 50% solids fluorothermoplastic aqueous dispersion. It is a melt-processable copolymer of tetrafluoroethylene and perfluorinated comonomers, with a melt viscosity several orders of magnitude lower than PTFE. Outstanding advantages associated with PTFE are:excellent chemical resistancewide service temperature rangenon-stick propertiesoutstanding soil-and-dirt repellencyextremely high weathering resistancenonflammableexcellent dielectric propertiesInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D792
Density 1.43 g/cc
0.0517 lb/in³
of dispersion; ASTM D1298
Solids Content 50 %
50 %
ASTM D4441
Particle Size 0.235 µm
0.235 µm
pH <= 7.0
<= 7.0
ASTM E70
Melt Index of Compound 15 g/10 min

@Load 5.00 kg,
Temperature 372 °C
15 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
ASTM D4591
Descriptive Properties Value Comments
Surface Active Ingredients non-ionic