Material Notes:
3M™ Dyneon™ Fluoroplastic Powder PFA 6503PBZ is a fluorothermoplastic powder with excellent thermal stability characteristics, designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tank liners, electrical insulation and low friction applications.Features and Benefits:Excellent thermal stabilityExcellent electrostaticsExcellent non-stick performanceOutstanding flow and fluidizationExcellent stress crack resistanceSmooth surfacesProcess targets: powder coatingNon-wettingHeat resistant to 260°C (500°F)Low frictionGood transparencyChemical resistantThis product complies with 21 CFR 177.1550 FDA regulationsInformation provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D792
Bulk Density 0.800 g/cc
0.0289 lb/in³
DIN 53466
Particle Size 30 µm
30 µm
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 372 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 380 %
380 %
ASTM D638
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 308 °C
586 °F
ASTM D4591
Maximum Service Temperature, Air 260 °C
500 °F
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent, but thickness not quantified