Material Notes:
Dynamar FX 5902A is a free-flowing fluoropolymer based processing additive that is designed for use at very low levels to improve processing of thermoplastics. At the very low use levels (typically 200-1000 ppm) necessary to improve processing, it does not alter or detract from good physical properties associated with high strength plastics.Features and BenefitsBroadens extrusion processing capabilities of polyolefin resinsIdeal for use in polyolefin resins containing antiblocking agents, pigments, and other inorganic additivesReduces or eliminates die build-upLowers apparent melt viscosityFor use at very low levelsFree-flowing fluoropolymer based processing aidCan offer performance and cost advantagesInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
Particle Mesh Size <= 10 Mesh
<= 10 Mesh
Descriptive Properties Value Comments
Active Ingredients (%) 97
Color White to off-white
Form Granular
Inorganic Additives % 3