Material Notes:
3M™ Dyneon™ Fluoroelastomer FG 5630Q can be compounded using standard water cooled internal mixers or two-roll mills. The “dry” ingredients should be blended before adding to the masticated gum. For best results, FG 5630Q should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks display excellent processing characteristics and storage stability.Composition: Di-polymer of vinylidene fluoride and hexafluoropropyleneIn compliance with FDA 21 CFR 177.2600When compared to diamine cured compounds this product gives excellent mold release, better mold flow, superior compression set resistance, and superior water resistance at elevated temperaturesProprietary incorporated cure technologyInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 30

@Temperature 121 °C
30

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 14.8 MPa
2140 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 210 %
210 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.00558 GPa
0.810 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 13 %
13 %
Aged 70 hours @ 200°C
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Opaque Off-White
MH, Maximum Torque 21.3 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque 1 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Solubility Ketones and Esters
t`50, Time to 50% cure 1.7 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure 2.8 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min 1.5 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C