Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ FEP 6307Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules

Category Polymer , Thermoplastic , Fluoropolymer , FEP
Manufacturer 3M Dyneon™
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ FEP 6307Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dyneon FEP 6307Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical propertiesHigh thermal stabilityLong term temperature rating up to 200°COutstanding chemical resistanceWide processing windowInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D792
Melt Index of Compound 7.0 g/10 min

@Load 5.00 kg,
Temperature 372 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.580 GPa
84.1 ksi
ASTM D790
Izod Impact, Notched NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D4591
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant <= 2.15

@Frequency 1000 - 1.00e+6 Hz
<= 2.15

@Frequency 1000 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 102 kV/mm
2590 kV/in
4.5 mil film; ASTM D149
Dissipation Factor <= 0.00030

@Frequency 1000 Hz
<= 0.00030

@Frequency 1000 Hz
ASTM D150
<= 0.00070

@Frequency 1e+6 Hz
<= 0.00070

@Frequency 1e+6 Hz
ASTM D150
Users viewing this material also viewed the following: