Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Controltac™ 3690C Graphic Film with Comply™ Adhesive

Category Polymer , Film
Manufacturer 3M
Trade Name Controltac™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Controltac™ 3690C Graphic Film with Comply™ Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a 2-mil white, clear or black film for screen printing graphics. The aggressive, pressure activated-adhesive is slideable and repositionable, and has air release channels for fast and easy bubble-free application. The film is well suited for graphics applied to sand cast, moderately rough surfaces and some low surface energy materials. Designed with a gray pigmented adhesive for good hiding power, this permanent film provides long term durability in severe weather and handling conditions encountered by commercial and industrial graphics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 MPa
2490 psi
Peel Strength 0.526 - 1.05 kN/m
3.00 - 6.00 pli
Adhesion to Powder coat paint
0.877 kN/m
5.00 pli
Adhesion to ABS
0.877 kN/m
5.00 pli
Adhesion to Acrylic enamel
0.877 kN/m
5.00 pli
Adhesion to Aluminum, etched
0.877 kN/m
5.00 pli
Adhesion to Chrome
0.877 kN/m
5.00 pli
Adhesion to Fiberglass
1.05 kN/m
6.00 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 32.0 °C
89.6 °F
Minimum Service Temperature, Air 4.00 °C
39.2 °F