Material Notes:
Scotch® ATG Gold Adhesive Transfer Tape 908 is .002" (0.05 mm) thick, acid free, pressure sensitive, permanent adhesive transfer tape.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Tape
76.2 microns
3.00 mil
Release Liner
Mechanical Properties Metric English Comments
Peel Strength 0.657 kN/m
3.75 pli
72 hr dwell, 180° peel at 12 in/min, 2 mil Al to Stainless Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 66.0 °C
151 °F
Long term
82.0 °C
180 °F
Short term
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Adhesive Type 320AF
Appearance Clear
Liner White paper with printed red 3M logo