3M 9579 Double Coated Tape with Adhesive 760

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9579 Double Coated Tape with Adhesive 760.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Double Coated Tape 9579 with 3M™ Adhesive 760 is a high-tack, hand-tearable, double coated film tape with a pressure sensitive adhesive on each side of the carrier. The medium firm adhesive features very high adhesion to a variety of surfaces, very good shear holding power and offers one-piece removal from most substrates.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Faceside Adhesive
76.2 microns
3.00 mil
Carrier
76.2 microns
3.00 mil
Backside Adhesive
102 microns
4.00 mil
Liner Caliper
229 microns
9.00 mil
Tape Caliper
Mechanical Properties Metric English Comments
Peel Strength 0.745 kN/m
4.25 pli
HDPE, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.877 kN/m
5.00 pli
Stainless Steel, 90°, 15 min RT; ASTM D3330
0.877 kN/m
5.00 pli
Polyester, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.8984 kN/m
5.125 pli
Stainless Steel, 90°, 72 hr RT; ASTM D3330
0.920 kN/m
5.25 pli
Stainless Steel, 90°, 72 hr at 70°C; ASTM D3330
1.10 kN/m
6.25 pli
Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
1.2600 kN/m
7.1875 pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Long term
66.0 °C
151 °F
Short term
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance White
Liner White, 62# Densified Kraft