3M 9088 High Performance Double Coated Tapes with Adhesive 375

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9088 High Performance Double Coated Tapes with Adhesive 375.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low surface energy substrates. The excellent initial tack ensures that a bond of good integrity is achieved soon after applicationInformation provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Liner Caliper
211 microns
8.30 mil
Total Thickness
Mechanical Properties Metric English Comments
Peel Strength 0.701 kN/m
4.00 pli
HDPE, 180° Peel, 2-mil Al Backing; ASTM D3330
1.1066 kN/m
6.3125 pli
High Pressure Laminate, 180° Peel, 2-mil Al Backing; ASTM D3330
1.3038 kN/m
7.4375 pli
ABS, 180° Peel, 2-mil Al Backing; ASTM D3330
1.40 kN/m
8.00 pli
Glass, 180° Peel, 2-mil Al Backing; ASTM D3330
1.5010 kN/m
8.5625 pli
Stainless Steel, 180° Peel, 2-mil Al Backing; ASTM D3330
1.6982 kN/m
9.6875 pli
Polycarbonate, 180° Peel, 2-mil Al Backing; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Continuous
150 °C
302 °F
Short Term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Carrier Polyester 0.5 mils
Adhesive Type Modified Acrylic
Appearance Clear
White Paper (Glassine) with Red 3M Logo