3M 901 Repulpable Forms-Splicing Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 901 Repulpable Forms-Splicing Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Repulpable Forms-Splicing Tape 901 is a semi-bleached kraft paper coated with a light green repulpable adhesive.Information provided by 3M
Physical Properties Metric English Comments
Thickness 114 microns
4.50 mil
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 70.5 MPa
10200 psi
Film Tensile Strength at Break, TD 27.6 MPa
4000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Descriptive Properties Value Comments
Adhesive Type Light green repulpable
Appearance White