Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7904 Screen Printable Sheet Vinyl Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7904 Screen Printable Sheet Vinyl Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utilizes 3M™ Adhesive 350, which is designed to permanently bond to high and low surface energy plastics, textured and contoured surfaces, powder coatings, and slightly oily metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 45.7 microns
1.80 mil
Adhesive
86.4 microns
3.40 mil
Facestock
170 microns
6.70 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.0877 kN/m
0.500 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.219 kN/m
1.25 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.219 kN/m
1.25 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.2410 kN/m
1.375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.2849 kN/m
1.625 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.29582 kN/m
1.6875 pli
Finely Textured Powder Coating, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.307 kN/m
1.75 pli
Finely Textured Powder Coating, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.307 kN/m
1.75 pli
Finely Textured Powder Coating, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3287 kN/m
1.875 pli
Finely Textured Powder Coating, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.351 kN/m
2.00 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.40538 kN/m
2.3125 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.40538 kN/m
2.3125 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.4163 kN/m
2.375 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.4163 kN/m
2.375 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.438 kN/m
2.50 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.4602 kN/m
2.625 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4602 kN/m
2.625 pli
Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4602 kN/m
2.625 pli
Smooth Powder Coating, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.47112 kN/m
2.6875 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.482 kN/m
2.75 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.482 kN/m
2.75 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.482 kN/m
2.75 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.49303 kN/m
2.8125 pli
Smooth Powder Coating, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.49303 kN/m
2.8125 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.526 kN/m
3.00 pli
Aluminum, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.53686 kN/m
3.0625 pli
Smooth Powder Coating, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.53686 kN/m
3.0625 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.5478 kN/m
3.125 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.5478 kN/m
3.125 pli
Aluminum, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.55877 kN/m
3.1875 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.570 kN/m
3.25 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.570 kN/m
3.25 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.58068 kN/m
3.3125 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.58068 kN/m
3.3125 pli
Smooth Powder Coating, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.60259 kN/m
3.4375 pli
Smooth Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.64642 kN/m
3.6875 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.64642 kN/m
3.6875 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.64642 kN/m
3.6875 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.657 kN/m
3.75 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.66833 kN/m
3.8125 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.66833 kN/m
3.8125 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.69024 kN/m
3.9375 pli
Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.701 kN/m
4.00 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.71216 kN/m
4.0625 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.7231 kN/m
4.125 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.75598 kN/m
4.3125 pli
Aluminum, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.75598 kN/m
4.3125 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.75598 kN/m
4.3125 pli
Aluminum, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.77789 kN/m
4.4375 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.789 kN/m
4.50 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.79981 kN/m
4.5625 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.8108 kN/m
4.625 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.8108 kN/m
4.625 pli
Aluminum, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.8108 kN/m
4.625 pli
Aluminum, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.82172 kN/m
4.6875 pli
Smooth Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.833 kN/m
4.75 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.88746 kN/m
5.0625 pli
Smooth Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.8984 kN/m
5.125 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.964 kN/m
5.50 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
Users viewing this material also viewed the following: