3M 7848 Laser Markable Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7848 Laser Markable Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Laser Markable Label Material 7847 and 7848 are specialty film label materials where a laser can ablate the top layer of a dual-layer facestock to create an image. The same laser can also kiss cut the label to size, maximizing flexibility for producing variable labels for durable applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 10.2 microns
0.400 mil
Facestock, Top layer
30.5 microns
1.20 mil
Adhesive
50.8 microns
2.00 mil
Facestock, Base layer
81.3 microns
3.20 mil
Liner
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
300mm/min; DIN 53455/ISO 527
Elongation at Break 13 %
13 %
DIN 53455/ISO 527
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type #350 high-holding acrylic
Liner Densified Kraft