3M 7710 Acetate Identification Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7710 Acetate Identification Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Label Material 7710 gloss clear acetate with 3M™ 400 high tack acrylic adhesive offers consistent, high quality appearance and excellent UV resistance. The transparent film easily die-cuts which helps extend die life in comparison with polyester label stocks. When used as an overlaminate, it provides depth, protection and rigidity as well as enhancing the appearance of the underlying label.Information provided by 3M
Physical Properties Metric English Comments
Thickness 20.3 microns
0.800 mil
Adhesive
63.5 microns
2.50 mil
Liner
76.2 microns
3.00 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.263 kN/m
1.50 pli
Polypropylene, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.263 kN/m
1.50 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 66°C; ASTM D3330
0.27391 kN/m
1.5625 pli
Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.3287 kN/m
1.875 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.4602 kN/m
2.625 pli
ABS, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.482 kN/m
2.75 pli
ABS, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.526 kN/m
3.00 pli
ABS, 180° Peel, Conditioned for 3 days at 66°C; ASTM D3330
0.5478 kN/m
3.125 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 66°C; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 77.0 °C
171 °F
Service
Minimum Service Temperature, Air -26.0 °C
-14.8 °F
Service
-12.0 °C
10.4 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 400 high tack acrylic
Liner 43# densified kraft