Material Notes:
3M™ General Purpose Vinyl Tape 764 can be used in non-critical applications such as color coding, bundling and safety marking, etc.Information provided by 3M
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.24 MPa
2645 psi
ASTM D3759
Elongation at Break 180 %
180 %
ASTM D3759
Peel Strength 0.1972 kN/m
1.125 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 29.0 °C
84.2 °F
Minimum Service Temperature, Air 16.0 °C
60.8 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Yellow, white, red, black, blue, transparent, green, orange, purple, gray, brown
Users viewing this material also viewed the following: