3M 7604FP Primalyn™ White Vinyl Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7604FP Primalyn™ White Vinyl Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Primalyn™ White Vinyl Label Material 7604FP is a flexible vinyl providing excellent squeeze bottle performance with consistent printability. This material utilizes 3M™ Adhesive 300, which has excellent quick tack and also bonds well to a variety of surfaces including LSE plastics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 20.3 microns
0.800 mil
Adhesive
81.3 microns
3.20 mil
Liner
88.9 microns
3.50 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.2410 kN/m
1.375 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.3287 kN/m
1.875 pli
HDPE, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.351 kN/m
2.00 pli
Polycarbonate, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.394 kN/m
2.25 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
HDPE, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.6355 kN/m
3.625 pli
Stainless Steel, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.64642 kN/m
3.6875 pli
Polycarbonate, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
0.82172 kN/m
4.6875 pli
Polypropylene, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 79.0 °C
174 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
10.0 °C
50.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type #300 Acrylic
Liner 55# Densified kraft