Material Notes:
3M™ 7300 Series Masking Film is a high performance, high temperature wide area masking film that is soft flexing for good drape and conformability.Information provided by 3M
Physical Properties Metric English Comments
Thickness 86.4 microns
3.40 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.1 MPa
2190 psi
ASTM D3756
Elongation at Break 680 %
680 %
ASTM D3756
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
for 60 mins
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type None
Appearance Translucent