3M 5498 PTFE Film Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 5498 PTFE Film Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ PTFE Film Tape 5498 has a film backing with a non-silicone rubber adhesive.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; ASTM D3752
102 microns
4.00 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.2 MPa
4820 psi
ASTM D3759
Elongation at Break 105 %
105 %
ASTM D3759
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Brown