3M™ Sandblast Stencil 507, also know as butter cut, is a general purpose sandblast stencil used for hand-cut and die-cut applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 1140 microns
45.0 mil
ASTM D3752
Mechanical Properties Metric English Comments
Peel Strength 0.49303 kN/m
2.8125 pli
Adhesion to Granite; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Dark green