3M 477 Vinyl Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 477 Vinyl Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Vinyl Tape 477 is comprised of a conformable, transparent vinyl backing with a versatile rubber adhesive. It is an excellent tape to use where abrasion resistance, transparency, conformability and moderate adhesion are needed.Information provided by 3M
Physical Properties Metric English Comments
Thickness 152 microns
6.00 mil
Backing; ASTM D3652
183 microns
7.20 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.3 MPa
3380 psi
ASTM D3574
Elongation at Break 230 %
230 %
ASTM D3759
Peel Strength 0.263 kN/m
1.50 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Transparent