Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 3939 Duct Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 3939 Duct Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Duct Tape 3939 is composed of waterproof polyethylene film over cloth scrim backing with a rubber adhesive used for demanding duct tape applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 229 microns
9.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.04 MPa
2762 psi
ASTM D3756
Elongation at Break 17 %
17 %
ASTM D3756
Peel Strength 0.60259 kN/m
3.4375 pli
to Steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Silver
Users viewing this material also viewed the following: