Foil/PET laminate. Tear resistance. Roof and gutter repair tape.Information provided by 3M
Physical Properties Metric English Comments
Thickness 63.5 microns
2.50 mil
Backing; ASTM D3652
114 microns
4.50 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.1 MPa
7120 psi
ASTM D3759
Peel Strength 0.5478 kN/m
3.125 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic
Users viewing this material also viewed the following: