3M 2A826 High Performance Temporary Surface Protection Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 2A826 High Performance Temporary Surface Protection Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ High Performance Temporary Surface Protection Tape 25A826 is a medium adhesion temporary protection tape designed for a variety of surface protection application.Information provided by 3M
Physical Properties Metric English Comments
Thickness 63.5 microns
2.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D3759
Elongation at Break 600 %
600 %
ASTM D3759
Peel Strength 0.07669 kN/m
0.4375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic-Based
Appearance Clear