Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 2929 General Use Duct Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 2929 General Use Duct Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Duct Tape 2929 is a utility grade, conformable cloth duct tape made with polyethylene film over cloth scrim and rubber adhesive. A good choice for temporary repairs, sealing, holding, and marking.Information provided by 3M
Physical Properties Metric English Comments
Thickness 140 microns
5.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.8 MPa
3450 psi
ASTM D3756
Elongation at Break 14 %
14 %
ASTM D3756
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Silver
Users viewing this material also viewed the following: