3M 1900 Specialty High Temperature Masking Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 1900 Specialty High Temperature Masking Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Value Duct Tape 1900 is a conformable cloth duct tape made with polyethylene film over cloth scrim and rubber adhesive. A good choice for non-critical applicationsInformation provided by 3M
Physical Properties Metric English Comments
Thickness 147 microns
5.80 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.7 MPa
3290 psi
ASTM D3756
Elongation at Break 15 %
15 %
ASTM D3756
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Synthetic rubber
Appearance Silver