Total 1285 HDPE film |
High Density Polyethylene (HDPE), Film Grade |
|
Total 2285 HDPE Bimodal Film Resin |
High Density Polyethylene (HDPE), Film Grade |
|
Total 2287 HDPE Bimodal Film Resin |
High Density Polyethylene (HDPE), Film Grade |
|
Total 3802 B HDPE, cable, sheet, pipe, injection molding |
High Density Polyethylene (HDPE), Pipe Grade |
|
Total 3802 Blue MDPE pipe, injection molding |
High Density Polyethylene (HDPE), Pipe Grade |
|
Total 49080 UV HDPE blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 50100.1 HDPE blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 50100.2 HDPE blow molding, sheet, thermoforming resin |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 5202 HDPE, blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 5202LD HDPE, blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 54050 HDPE, blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 5502 BZ HDPE injection blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 5502 HDPE, blow molding, pipe |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 6410 HDPE Film Resin |
High Density Polyethylene (HDPE), Film Grade |
|
Total 8183 HDPE, blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total 9458 HDPE Film Grade |
Medium Density Polyethylene (MDPE), Film Grade |
|
Total CD 4300 HDPE extrusion |
High Density Polyethylene (HDPE), Extruded |
|
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film |
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade |
EVA
|
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film |
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade |
EVA
|
Total EVA 1005 VN 35 Ethylene Vinyl Acetate Copolymer - Blown Film |
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade |
EVA
|
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film |
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade |
EVA
|
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film |
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade |
EVA
|
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film |
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade |
EVA
|
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film |
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade |
EVA
|
Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film |
Ethylene Vinyl Acetate Copolymer (EVA), Film Grade |
EVA
|
Total FE 8000 LDPE blown film |
Low Density Polyethylene (LDPE), Film Grade |
|
Total FE 8004 LDPE blown film |
Low Density Polyethylene (LDPE), Film Grade |
|
Total HDPE 2008 SN 60 High Density Polyethylene - Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE 51090 High Density Polyethylene - Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE 53090 High Density Polyethylene - Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE 5502 R3 High Density Polyethylene - Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE 56020 S High Density Polyethylene - Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin |
High Density Polyethylene (HDPE), Injection Molded |
HDPE
|
Total HDPE 6420 High Density Polyethylene, Film Resin |
High Density Polyethylene (HDPE), Film Grade |
HDPE
|
Total HDPE HD 6221 High Density Polyethylene - Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE HL 535 High Density Polyethylene, Film Resin |
High Density Polyethylene (HDPE), Film Grade |
HDPE
|
Total HDPE HL 717 High Density Polyethylene - Blown Film |
High Density Polyethylene (HDPE), Film Grade |
HDPE
|
Total HDPE MS201 BN-NA High Density Polyethylene - Fuel Tank Resin |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE SB 1359 High Density Polyethylene - Injection Stretch Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE SB 1461 High Density Polyethylene - Injection Stretch Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
HDPE
|
Total HDPE XLS 12 B High Density Polyethylene - Pipes and Fittings |
High Density Polyethylene (HDPE), Pipe Grade |
HDPE
|
Total HDPE XT10 N High Density Polyethylene - Pipe Resin |
High Density Polyethylene (HDPE), Pipe Grade |
HDPE
|
Total HDPE XT10B High Density Polyethylene, Pipe Resin |
High Density Polyethylene (HDPE), Pipe Grade |
HDPE
|
Total HDPE XT25N High Density Polyethylene, Pipe Resin |
High Density Polyethylene (HDPE), Pipe Grade |
HDPE
|
Total HL 428 HDPE film resin |
High Density Polyethylene (HDPE), Film Grade |
|
Total HP 401N Natural HDPE, pipe |
High Density Polyethylene (HDPE), Pipe Grade |
|
Total Impact Polystyrene 940E Super High Impact Polystyrene, Sheet Extrusion and Thermoforming Grade |
Polystyrene, Impact Modified |
Impact Polystyrene
|
Total L425 HDPE Film |
Medium Density Polyethylene (MDPE), Film Grade |
|
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film |
Low Density Polyethylene (LDPE), Film Grade |
LDPE
|
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding |
Low Density Polyethylene (LDPE), Molded |
LDPE
|
Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding |
Low Density Polyethylene (LDPE), Molded |
LDPE
|
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding |
Low Density Polyethylene (LDPE), Molded |
LDPE
|
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating |
Low Density Polyethylene (LDPE), Extrusion Grade |
LDPE
|
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating |
Low Density Polyethylene (LDPE), Extrusion Grade |
LDPE
|
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film |
Linear Low Density Polyethylene (LLDPE), Film Grade |
LLDPE
|
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film |
Linear Low Density Polyethylene (LLDPE), Film Grade |
LLDPE
|
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film |
Linear Low Density Polyethylene (LLDPE), Film Grade |
LLDPE
|
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film |
Linear Low Density Polyethylene (LLDPE), Film Grade |
LLDPE
|
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film |
Linear Low Density Polyethylene (LLDPE)/Butene, Film |
Lotrene®
|
Total Lotrene® Q2018C Linear Low Density Polyethylene, Blown Film |
Linear Low Density Polyethylene (LLDPE)/Butene, Film |
Lotrene®
|
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film |
Linear Low Density Polyethylene (LLDPE)/Butene, Film |
Lotrene®
|
Total Lumicene® M 3410 EP HDPE Film, sheet |
Medium Density Polyethylene (MDPE), Film Grade |
Lumicene®
|
Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding |
Medium Density Polyethylene (MDPE), Rotational Molded |
Lumicene®
|
Total Lumicene® mPE M 4040 Metallocene Polyethylene, Cast Film |
Medium Density Polyethylene (MDPE), Film Grade |
Lumicene®
|
Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding |
Medium Density Polyethylene (MDPE), Rotational Molded |
Lumicene®
|
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film |
High Density Polyethylene (HDPE), Film Grade |
Lumicene®
|
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
Lumicene®
|
Total Lumicene® mPE M5220 M Metallocene High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Lumicene®
|
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Lumicene®
|
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film |
High Density Polyethylene (HDPE), Film Grade |
Lumicene®
|
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film |
High Density Polyethylene (HDPE), Film Grade |
Lumicene®
|
Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene |
Polypropylene (PP) |
Lumicene®
|
Total Lumicene® MR 2002 Polypropylene, Metallocene Polypropylene |
Polypropylene (PP) |
Lumicene®
|
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding |
Polypropylene, Molded |
Lumicene®
|
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding |
Polypropylene, Molded |
Lumicene®
|
Total Lumicene® MR30MC2 Metallocene Random Copolymer Polypropylene, Injection Molding |
Polypropylene, Molded |
Lumicene®
|
Total Lumicene® MR30MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding |
Polypropylene, Molded |
Lumicene®
|
Total Lumicene® MR60MC2 Metallocene Random Copolymer Polypropylene, Injection Molding |
Polypropylene, Molded |
Lumicene®
|
Total MDPE 3802 B Medium Density Polyethylene, Cable |
MDPE |
MDPE
|
Total MDPE 3802 B Medium Density Polyethylene, Pipes & Fittings |
MDPE |
MDPE
|
Total MDPE 3802 Blue Medium Density Polyethylene, Stripes |
MDPE |
MDPE
|
Total MDPE 3802 Medium Density Polyethylene, Blow Molding |
Medium Density Polyethylene (MDPE), Molded |
MDPE
|
Total MDPE 3802 Medium Density Polyethylene, Cable |
Medium Density Polyethylene (MDPE), Extruded |
MDPE
|
Total MDPE 3802 YCF Medium Density Polyethylene, Pipes & Fittings |
MDPE |
MDPE
|
Total MDPE HF 513 Medium Density Polyethylene, Blown Film |
Medium Density Polyethylene (MDPE), Film Grade |
MDPE
|
Total MDPE HL 323 Medium Density Polyethylene, Film Resin |
Medium Density Polyethylene (MDPE), Film Grade |
MDPE
|
Total MDPE HR 515 Medium Density Polyethylene, Blown Film |
Medium Density Polyethylene (MDPE), Film Grade |
MDPE
|
Total MDPE LF 38 YS CF Medium Density Polyethylene, Stripes |
MDPE |
MDPE
|
Total MS 201 B HDPE blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total MS 201 B N HDPE blow molding |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene |
Polystyrene, Impact Modified |
Polystyrene Impact
|
Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene |
Polystyrene, Impact Modified |
Polystyrene Impact
|
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene |
Polystyrene, Impact Modified |
Polystyrene Impact
|
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding |
Polypropylene, Molded |
PPC
|
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding |
Polypropylene, Molded |
PPC
|
Total PPC 11712 Polypropylene, Heterophasic Copolymer |
Polypropylene (PP) |
|
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding |
Polypropylene, Molded |
PPC
|
Total PPC 3660 Polypropylene, Heterophasic Copolymer |
Polypropylene (PP) |
|
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion |
Polypropylene, Extrusion Grade |
PPC
|