Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Renegade Materials Corporation > Category : Filled/Reinforced Thermoset Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric Filled/Reinforced Thermoset
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ IM7 12K Carbon Unitape Carbon Fiber/Thermoset Composite
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ S2-Glass Fabric Filled/Reinforced Thermoset
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric Filled/Reinforced Thermoset
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric Carbon Fiber/Thermoset Composite
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) 6781 S2 Glass Fabric Filled/Reinforced Thermoset
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) Resin Filled/Reinforced Thermoset
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin Filled/Reinforced Thermoset
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III Filled/Reinforced Thermoset
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin IM7 12K Carbon Uni-tape Filled/Reinforced Thermoset
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric Filled/Reinforced Thermoset
Renegade Materials Corporation RM-3006 Bismaleimide (BMI) Paste Adhesive Filled/Reinforced Thermoset
Renegade Materials Corporation RM-3010 Bismaleimide (BMI) Resin for VARTM Filled/Reinforced Thermoset
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 3K 8HS Fabric Filled/Reinforced Thermoset
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 6781 S2 Glass Fabric Filled/Reinforced Thermoset
Renegade Materials Corporation RM-5003 Cyanate Ester Prepreg 4581 Quartz Fabric Filled/Reinforced Thermoset
Copyright © lookpolymers.com All Rights Reserved