Radici Group Plastics
Radici Group Plastics > Polyethylene (PE)
Manufacturer :
Radici Group Plastics
>
Category :
Polyethylene (PE)
Product List
Tips:
100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Category
Trade Name
Radici Radilene® R 30 IE 0 3036 B Low Density Polyethylene
LDPE
Radici Radilene® R 70 IE 0 2060 C High Density Polyethylene
HDPE
Radici Radilene® R 70 IE 5058 B High Density Polyethylene
HDPE
Radici Radilene® R 70 IF 0 4058 A High Density Polyethylene
HDPE