PRODUCT NO. Category Trade Name
Polyram RamTough PZ324G4NT Polycarbonate, 20% Glass Fiber, Flame Retardant Polycarbonate, Glass Fiber Filled, Flame Retardant
Polyram RamTough PZ333G2 Polycarbonate, 10% Glass Fiber, Flame Retardant Polycarbonate, Glass Fiber Filled, Flame Retardant
Polyram RamTough RZ321G2 Polycarbonate, 10% Glass Fiber, Flame Retardant Polycarbonate, Glass Fiber Filled, Flame Retardant
Polyram RamTough RZ320G2 Polycarbonate, 10% Glass Fiber, Flame Retardant Polycarbonate, Glass Fiber Filled, Flame Retardant