Loxim Industries
Loxim Industries > Nylon
Manufacturer :
Loxim Industries
>
Category :
Nylon
Product List
Tips:
100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Category
Trade Name
Loxim 300 00HB Nylon 6
Nylon 6, Unreinforced, Flame Retardant
Loxim 300 00V0 Nylon 6
Nylon 6, Unreinforced, Flame Retardant
Loxim 315 01HB Nylon 6
Nylon 6, Glass Fiber Filled, Flame Retardant
Loxim 315 01V0 Nylon 6
Nylon 6, Glass Fiber Filled, Flame Retardant
Loxim 315 02HB Nylon 6
Nylon 6, Glass Fiber Filled, Flame Retardant
Loxim 330 01HB Nylon 6
Nylon 6, Glass Fiber Filled, Flame Retardant
Loxim 330 01HSL Nylon 6
Nylon 6, Glass Fiber Filled, Flame Retardant
Loxim 330 01V0 Nylon 6
Nylon 6, Glass Fiber Filled, Flame Retardant
Loxim 330 12HSL Nylon 6
Nylon 6, Glass Fiber Filled, Flame Retardant
Loxim 330 12V0 Nylon 6
Nylon 6, Glass Fiber Filled, Flame Retardant
Loxim 340 01HB Nylon 6
Nylon 6, 40% Glass Fiber Filled
Loxim 430 01HB Nylon 6,6
Nylon 66, Glass Fiber Filled, Flame Retardant
Loxim 433 01HB Nylon 6,6
Nylon 66, Glass Fiber Filled, Flame Retardant
Loxim 400 00HB Nylon 6,6
Nylon 66, Unreinforced, Flame Retardant