Lehmann & Voss LUVOCOM® 1-1109 Polyamide 66, with glass fiber and PTFE, heat stabilized |
Nylon 66, Glass Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-1114 Polyamide 66, with carbon fiber, low-warpage, heat stabilized |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity |
Nylon 66, PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7004 Polyamide 66, with glass fiber and carbon fiber, heat stabilized |
Nylon 66, Glass/Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized |
Nylon 66, Aramid Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7177 Polyamide 66, with PTFE, lubricant modified, heat stabilized |
Nylon 66, PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7305/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized |
Nylon 66, Glass/Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7332/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized |
Nylon 66, Carbon Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7390 Polyamide 66, with carbon fiber, PTFE, lubricant modified |
Nylon 66, Carbon Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized |
Nylon 66, Carbon Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7488 Polyamide 66, with carbon fiber, heat stabilized |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7532 Polyamide 66, with carbon fiber |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized |
Nylon 66, Carbon Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7791 Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized |
Nylon 66, Carbon Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7805 Polyamide 66, with glass fiber, aramid reinforcement and PTFE |
Nylon 66, Glass Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7882 Polyamide 66, with carbon fiber and PTFE, heat stabilized |
Nylon 66, Carbon Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7968 Polyamide 66, with PTFE, lubricant modified |
Nylon 66, PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-7985 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized |
Nylon 66, Aramid Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8064 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized |
Nylon 66, Carbon Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8070 VP Polyamide 66, with carbon fiber, lubricant modified, heat stabilized |
Nylon 66, Carbon Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66, with carbon fiber, toughness-modified |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8218 Polyamide 66, with carbon fiber, toughness-modified |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized |
Nylon 66, Glass/Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE |
Nylon 66, PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized |
Nylon 66, Glass Fiber/PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8520 Polyamide 66, with carbon fiber, toughness-modified |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-8521 Polyamide 66, with carbon fiber and glass fiber |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19/XCF/20 Polyamide 46, with carbon fiber |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber |
Nylon 46, Glass Fiber Reinforced |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7278 Polyamide 46, with carbon fiber |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber |
Nylon 46, Glass Fiber Reinforced |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7330 Polyamide 46, with PTFE, lubricant modified |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7416 Polyamide 46, with carbon fiber and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7652 Polyamide 46, with PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7660 Polyamide 46, with glass fiber, PTFE, lubricant modified |
Nylon 46, Lubricated + Glass Fiber Reinforced |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7669 Polyamide 46, with glass fiber and PTFE |
Nylon 46, Lubricated + Glass Fiber Reinforced |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7744 Polyamide 46, with aramid reinforcement and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7748 Polyamide 46, with carbon fiber, PTFE, lubricant modified |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7810 Polyamide 46, with aramid reinforcement and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7827 Polyamide 46, with PTFE, easy flowing |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7950 Polyamide 46, with aramid reinforcement and PTFE, toughness-modified, easy flowing |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-7969 Polyamide 46, with aramid reinforcement and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8043 Polyamide 46, with PTFE, lubricant modified, high viscosity |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8195/FR Polyamide 46, with carbon fiber |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8250 Polyamide 46, lubricant modified |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8263 Polyamide 46, with carbon fiber and glass fiber, lubricant modified |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 19-8373 Polyamide 46, with carbon fiber, lubricant modified |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1-RG 2 Polyamide 66, with carbon fiber, heat stabilized |
Nylon 66, 10% Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 1t-7503 Polyamide 6/6T, with PTFE, lubricant modified |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 21-7976 Polyamide 6/6T, with glass fiber and PTFE, 8-mm-granulate |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 21-8113 Polyamide 6/6T, with carbon fiber, lubricant modified |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3/TF/20/BK Polyamide 6, with PTFE |
Nylon 6, PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-7088/GY7012 Polyamide 6, with carbon fiber and glass fiber, low-warpage |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-7234-1 Polyamide 6, with carbon fiber, electrically conducting |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-7281/PL/HI/BK Polyamide 6, with PTFE, toughness-modified |
Nylon 6, PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-7901 Polyamide 6, with glass fiber and carbon fiber |
Nylon 6, 10% Glass Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-8269 Polyamide 6, with basalt fiber |
Nylon 6, Mineral Reinforced, Impact Grade |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber |
Nylon 6, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced |
Nylon 6 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber |
Nylon 6, 10% Glass Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized |
Nylon 46 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber |
Nylon 12, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 6-7433 Polyamide 12, with carbon fiber, hydrolysis resistant |
Nylon 12, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 6-7595 Polyamide 12, with carbon fiber |
Nylon 12, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 6-7833 Polyamide 12, with PTFE, lubricant modified |
Nylon 12, PTFE Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 6-7834 Polyamide 12, lubricant modified |
Nylon 12 |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 6-8159 Polyamide 12, with carbon fiber |
Nylon 12, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 6-8395 Polyamide 12, with carbon fiber |
Nylon 12, Carbon Fiber Filled |
LUVOCOM®
|
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified |
Nylon 12, PTFE Filled |
LUVOCOM®
|