Manufacturer : Lehmann & Voss & Co. > Category : Nylon 610 Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Nylon 610, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 7-0755 Polyamide 610, with glass fiber and PTFE Nylon 610, Glass Reinforced LUVOCOM®