Ipiranga Petrochem > HDPE
Manufacturer :
Ipiranga Petrochem
>
Category :
HDPE
Product List
Tips:
100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Category
Trade Name
Ipiranga Petrochem GD 5150 K HDPE
HDPE
Ipiranga Petrochem GD 5160 HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GE 4960 BR HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GF 4950 HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GF 4950 HS HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GF 4960 HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GF 5250 HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GM 5010 T2 HDPE
High Density Polyethylene (HDPE), Pipe Grade
Ipiranga Petrochem GM 5240 PR HDPE
High Density Polyethylene (HDPE), Pipe Grade
Ipiranga Petrochem GM 7746 HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GM 8250 HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GM 8260 HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GM 9245 F HDPE
High Density Polyethylene (HDPE), Pipe Grade
Ipiranga Petrochem GP 9452 F HDPE
High Density Polyethylene (HDPE), Film Grade
Ipiranga Petrochem GV 0350 HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem HA 7260 HDPE
High Density Polyethylene (HDPE), Injection Molded
Ipiranga Petrochem HC 7260 HDPE
High Density Polyethylene (HDPE), Injection Molded
Ipiranga Petrochem HC 7260 LS HDPE
High Density Polyethylene (HDPE), Injection Molded
Ipiranga Petrochem HC 7260 LS-L HDPE
High Density Polyethylene (HDPE), Injection Molded
Ipiranga Petrochem HD 7255 LS-L HDPE
High Density Polyethylene (HDPE), Injection Molded
Ipiranga Petrochem HD 7555 LS-L HDPE
High Density Polyethylene (HDPE), Injection Molded
Ipiranga Petrochem HE 7250 LS-L HDPE
High Density Polyethylene (HDPE), Injection Molded
Ipiranga Petrochem GF 5150 HDPE
High Density Polyethylene (HDPE), Pipe Grade
Ipiranga Petrochem GM 5250 OC HDPE
High Density Polyethylene (HDPE), Pipe Grade
Ipiranga Petrochem GM 7040 G HDPE
High Density Polyethylene (HDPE), Pipe Grade
Ipiranga Petrochem GM 7746 A HDPE
High Density Polyethylene (HDPE), Blow Molding Grade
Ipiranga Petrochem GM 9450 F HDPE
High Density Polyethylene (HDPE), Film Grade
Ipiranga Petrochem GP 100 BK HDPE
HDPE
Ipiranga Petrochem GP 100 OR HDPE
HDPE