E-Polymers Co. Ltd. > Polyester, TP
Manufacturer :
E-Polymers Co. Ltd.
>
Category :
Polyester, TP
Product List
Tips:
100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Category
Trade Name
E-Polymers TEKALOY® F50G50 50% Glass Fiber Reinforced PBT/PET Alloy
PBT + PET Blend, Glass Filled
TEKALOY®
E-Polymers TEKALOY® S630XB Heat Resistance, Weatherability PC/PBT Alloy
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
TEKALOY®
E-Polymers TEKASTER® F100 low-mid viscosity PBT
Polybutylene Terephthalate (PBT)
TEKASTER®
E-Polymers TEKASTER® F101F Fast cycle time PBT
Polybutylene Terephthalate (PBT)
TEKASTER®
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT
Polybutylene Terephthalate (PBT), Flame Retardant
TEKASTER®
E-Polymers TEKASTER® F10G30 30% Glass Fiber Reinforced PBT
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
TEKASTER®
E-Polymers TEKASTER® F10G30FR 30% Glass Fiber Reinforced Flame Retardant PBT
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
TEKASTER®
E-Polymers TEKASTER® F10G30H 30% Glass Fiber Reinforced Impact Modified PBT
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
TEKASTER®
E-Polymers Tekaster® F615G30 , 30% Glass Fiber Reinforced PET
Polyethylene Terephthalate (PET), 30% Glass Reinforced
TEKASTER®
E-Polymers TEKASTER® F615G55 55% Glass Fiber Reinforced High Modulus PET
Polyethylene Terephthalate (PET), 60% Glass Reinforced
TEKASTER®
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET
Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
TEKASTER®
E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET
Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
TEKASTER®
E-Polymers Tekaloy® T80GFR , Flame Retardant, 30% Glass Fiber Reinforced PBT/ABS Alloy
ABS/Polyester Alloy + GF
TEKALOY®
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET
Polyethylene Terephthalate (PET), 50% Glass Reinforced
TEKASTER®
E-Polymers Tekaloy® S630X , High Impact, Weather Resistance, Chemical Resistance PC/PBT Alloy
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
TEKALOY®
E-Polymers Tekaloy® T80 , Dimensional Stability PBT/ABS Alloy
ABS/Polyester Alloy
TEKALOY®
E-Polymers Tekaloy® T80FR , Flame Retardant Un-Reinforced PBT/ABS Alloy
ABS/Polyester Alloy
TEKALOY®
E-Polymers Tekaloy® T80G20 , 20% Glass Fiber Reinforced PBT/ABS Alloy
ABS/Polyester Alloy + GF
TEKALOY®
E-Polymers TEKALOY® F50G30 30% Glass Fiber Reinforced PBT/PET Alloy
PBT + PET Blend, Glass Filled
TEKALOY®
E-Polymers Tekaloy® T80HI Impact Resistance PBT/ABS Alloy
ABS/Polyester Alloy
TEKALOY®
E-Polymers TEKASTER® F101M Unreinforced impact modified PBT
Polybutylene Terephthalate (PBT), Impact Grade
TEKASTER®