Manufacturer : Celanese Corporation > Category : Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
Celanese THERMX CG923 PCT, 20% Glass Reinforced Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced THERMX
Celanese Thermx® CG023 NC010 PCT Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced Thermx®
Celanese Thermx® CG923 BK010 PCT Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced Thermx®
Celanese Thermx® CG923 NC010 PCT Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced Thermx®
Celanese THERMX CG023 PCT, 20% Glass Reinforced Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced THERMX