Celanese Celanex® 6400 Polyester (PBT), 40% Glass/Mineral Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® 6407HR PBT, 30% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® 6500HF PBT, Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® 6500LM PBT, 30% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® 7305 Polyester (PBT), 35% Glass/Mineral Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® 7316 PBT, 35% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® 7700 Polyester (PBT), 35% Glass/Mineral Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® 7714 PBT, Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese CELANEX 6400-2 PBT, Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled CELANEX
Celanese CELANEX 6402R PBT, 40% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled CELANEX
Celanese CELANEX 6407 PBT, 30% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled CELANEX
Celanese CELANEX 6500 PBT, 30% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled CELANEX
Celanese CELANEX 6500HF PBT, Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled CELANEX
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® 6500HR PBT, Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese Celanex® J235 PBT, 35% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®
Celanese CELANEX 7716 PBT, 35% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled CELANEX
Celanese CELANEX J600 PBT, 40% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled CELANEX
Celanese CELANEX LW2547W PBT, 30% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled CELANEX
Celanese Celanex® LW2547W PBT, 30% Mineral / Glass Reinforced Polybutylene Terephthalate (PBT), Glass + Mineral Filled Celanex®