Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Celanese Corporation > Category : Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled Product List

Tips:100 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Category Trade Name
Celanese CELANEX 2300 GV1/50 PBT, 50% Glass Reinforced Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled CELANEX
Celanese Celanex® 3316CT PBT, 50% Glass Reinforced Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled Celanex®
Celanese Celanex® LW2333R PBT, 50% Specialty Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled Celanex®
Celanese Celstran® PBT-GF50-08 PBT, 50% Glass Reinforced Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled CELSTRAN