Celanese Impet® 610R Recycled PET, 13% Glass/Mineral Reinforced Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced Impet®
Celanese Impet® 840R Recycled PET, 45% Glass/Mineral Reinforced Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced Impet®
Celanese Impet® 320R Recycled PET, 15% Glass Reinforced Polyethylene Terephthalate (PET), Recycled, Glass Reinforced Impet®
Celanese Impet® 630R Recycled PET, 35% Glass/Mineral Reinforced Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced Impet®